0 Views 2026-09-17 09:11 PPOEM

Compare mould venting: A Practical Thermoforming Guide

This guide covers how to compare mould venting on a vacuum formed part: what the designer has to decide, what the mould maker needs to know, and the checks that catch problems before tooling is cut.

Compare mould venting: A Practical Thermoforming Guide

What it affects

The main effects are on wall thickness, cycle time and how much hand work the part needs after forming. On a thick gauge part these three decide the piece price, so the decision taken here shows up in every release afterwards.

Typical values

ItemValue
Sheet range1.5–12 mm for thick gauge work
Forming areaup to 3,000 × 2,000 mm
Formed tolerance±0.5 mm typical
Trimmed tolerance±0.2 mm on router cut edges
Draft angle3 degrees minimum, 5 degrees preferred
Corner radiusat least 3 × sheet thickness
Cycle time60–180 s depending on gauge and material

How it is controlled

  1. The sheet is formed over the mould with vacuum and, where the draw is deep, with plug assist.
  2. Drawings are reviewed and a manufacturability report is issued with wall thickness, draft and radii marked up.
  3. Tooling is cut: aluminium for production volumes, composite or printed moulds for samples and first articles.
  4. The part cools on a jig so the shape is held while the material stabilises.
  5. Trimming is done on 5-axis routers or with a dedicated trim fixture to meet the drawing.

thermoforming production control

Common mistakes

  • add ribs or returns instead of increasing sheet thickness to save weight and cycle time
  • call out the finish on the drawing: mould texture, paint, or as-formed gloss
  • keep a draft angle of at least 3 degrees on vertical walls so the part releases cleanly
  • plan the trim line on a flat face so the router can hold tolerance

How to specify it on the drawing

Put the decision on the drawing rather than in an email: state the material and grade, the gauge, the finish, the surfaces that must not carry marks, and the tolerance that applies to the trimmed edges. Where the part has to mate with another component, mark the datum faces so the trim fixture and the inspection report use the same reference. A drawing that states these points removes most of the questions that otherwise surface during sampling.

Checklist before tooling is cut

  • Material and grade fixed, including flame retardancy, UV or food contact requirements
  • Gauge selected from the load case, not from habit
  • Draft angle and corner radii checked against the sheet thickness
  • Trim line placed on a face the router can reach
  • Finish and colour standard agreed, with a reference if the colour is critical
  • Inspection points agreed and noted for the dimensional report

Related terms

  • Mould texture
  • Mould venting
  • Wall thickness distribution
  • Threaded inserts
  • Break even quantity
  • Nesting for trimming

Frequently asked questions

Does this change the tooling cost?

Yes. Decisions taken at drawing stage move the tooling cost more than any later change, which is why the manufacturability review is done before the tool is cut.

What information do you need to advise on it?

A 3D file, the material if it is fixed, the annual quantity and the finish. With those the answer comes back with a recommended route and a quotation.

Need a part like this?

Send the 3D file or drawing with your quantity — manufacturability review and quotation within 24 hours.

Get a Quote

Leave a Message